微颗粒成分对金属网布筛管的堵塞机理实验研究
邓福成1,2,5*,林海3,曹砚锋4,潘豪4,闫伟5
1 长江大学机械工程学院,荆州 424023 2 湖北省油气钻完井工具工程技术研究中心,荆州 424023 3 中海石油(中国)有限公司天津分公司,天津 300459 4 中海油研究总院,北京 100028 5 中国石油大学(北京)石油工程学院,北京 102249
Experimental study of plugging mechanisms of metal mesh screens with different particle compositions
DENG Fucheng1,2,5, LIN Hai3, CAO Yanfeng4, PAN Hao4, YAN Wei5
1 School of Mechanical Engineering, Yangtze University, Jingzhou 424023, China 2 Hubei Province Engineering Research Centers of Oil & Gas Drilling and Completion Tools, Jingzhou 424023, China 3 CNOOC China Limited, Tianjin Branch, Tianjin 300451, China 4 CNOOC Research Institute, Beijing 100028, China 5 College of Petroleum Engineering, China University of Petroleum-Beijing, Beijing 102249, China

全文:   HTML (1 KB) 
文章导读  
摘要  针对金属网布筛管被地层砂中微颗粒堵塞而造成低产或停产的情况,展开微颗粒对金属网布筛管堵塞机理的研究,提出微颗粒成分及出砂次序对金属网布筛管堵塞机理的影响。利用油气井防砂模拟实验装置模拟了微颗粒防砂过程中金属网布筛管的堵塞过程及堵塞机理,分析了影响金属网布筛管堵塞程度的因素及规律。结果表明:(1) 金属网布筛管对微颗粒中蒙脱石含量非常敏感,蒙脱石含量越高,堵塞越严重,产能下降越快,致使其产生严重堵塞的蒙脱石含量分界线为10%。(2)微颗粒混合组分越多,金属网布筛管堵塞速度越快,堵塞程度越严重;微颗粒组分为单一组分时,纯蒙脱石堵塞后的米采指数最小。(3)筛管外泥饼颗粒外粗内细、明显分层,说明黏土的水化膨胀性及泥饼的形成是造成金属网布筛管孔喉堵塞的重要原因。
服务
把本文推荐给朋友
加入我的书架
加入引用管理器
关键词 : 防砂微颗粒, 金属网布筛管, 堵塞, 泥质含量, 含砂量
Abstract

  The micro-particles in oil and gas reservoir sand can block the metal mesh used to stop sand particles entering the product stream, which will cause the production to decrease or shutdown. In order to help resolve these problems, this paper studied the mechanisms of micro-particles plugging metal mesh. The plugging mechanisms of metal mesh screen caused by different micro-particles compositions at different sand production sequences were put forward. The oil and gas well sand control simulation experimental device was used to study the plugging process, plugging mechanisms and effects of the metal mesh screen on the sand control process by micro-particles. The factors affecting the degree of plugging of the metal mesh screen was also studied here. The results show that: (1) The metal mesh screen plugging is very sensitive to the montmorillonite content of the micro-particles. The higher the montmorillonite content, the more rapidly the production capacity decreased. The boundary of the serious blockage of montmorillonite contents is 10%.  (2) The more components of the micro-particles, the faster the metal mesh screen was blocked, and the blockage was more serious. When the micro-particles are a single group, the oil well production index of the blocked screen pipe with pure montmorillonite is minimum. (3) The mud cake outside the screen is apparently layered. It shows that the hydration swelling characteristics of clay and the formation of the mud cake are two important factors that cause the pore throat blockage of the metal mesh screen.

Key words: micro-particles metal mesh screen plug montmorillonite content sand content
收稿日期: 2017-02-13     
PACS:    
基金资助:国家自然科学基金(51504040)、湖北省技术创新重大项目(2016ACA181)和长江青年基金(2015cqn43)联合资助
通讯作者: 邓福成, dengfucheng128@163.com
引用本文:   
邓福成,林海,曹砚锋,潘豪,闫伟. 微颗粒成分对金属网布筛管的堵塞机理实验研究[J]. 石油科学通报, 2017, 2(4): 500-506. DENG Fucheng, LIN Hai, CAO Yanfeng, PAN Hao, YAN Wei. Experimental study of plugging mechanisms of metal mesh screens with different particle compositions. Petroleum Science Bulletin, 2017, 2(4): 500-506.